Fig. 5From: Characteristics of diamond turned NiP smoothed with ion beam planarization techniqueAFM images (40 μm × 10 μm) of a diamond turned surface before and after one IBP run on sample A. The amplitudes of the tool marks were reduced from 20 nm to 2.5–4 nm (height scale 80 nm)Back to article page