Fig. 7From: Crystallization behavior of ion beam sputtered HfO2 thin films and its effect on the laser-induced damage thresholdArrhenius-plot of the crystallization times for the 15 (black), 20 (dark gray), and 50 nm layers (gray); a common activation energy was used in the fitting procedureBack to article page